CHARACTERISTICS:
Voltage: 4 to 6 V
stainless steel anode
Working time: between 30 and 60 seconds
Can be used with any metal
Working temperature: ambient.
PREPARATION:
Use a bottle with a capacity of 2 liters, mix 1.5 liters of distilled water and the total contents of the bottle supplied.
Shake vigorously until you notice an increase in temperature in the preparation.
Place in the work tank and add half a liter more of distilled water.